MIL-DTL-43695C
TABLE II. Classification of defects
Classification
Examine
Defect
Major
Minor
Finish
Area of no film:
(continued)
- bare metal showing in area more than
3 square inches
103
- bare metal showing in area
3 square inches or less
204
Note: Areas of no film on interior surfaces of
rectangular tubes, where slotted or
diagonally cut at end, and shank of
through rivets are allowed. Areas of
no film of ¼ inch or less are allowed on
inside of boss, purlin end fittings and in
area of brace pad adjacent to brace stud.
Area of no enamel 1/16 inch wide is allowed
at junction of riveted assemblies to tube.
Area of thin film:
primer shows through in area
9 square inches or more
104
- primer shows through in area less than
9 square inches
205
Scratch or scuff exposing bare metal:
- 12 inches or more in longest dimension
105
- less than 12 inches in longest dimension
206
Note: Defects in finish attributable to flexing
of movable joints during examination will
not be scored as a defect. However, the
supplier shall touch up areas of finish
damaged during flexing of movable joints.
Minor shade variations resulting from
touch up operations shall not be
considered a defect.
Coating thickness not as specified (see 1/)
106
Construction Any part of component not fabricated of
& workman- applicable reference materials
107
ship
Any component or part missing
108
Any component not fabricated as specified, e.g.:
- stud not capable of being turned within
the pad by hand operation without
having to use a tool for force
207
- end of hinge pin (item 8) not securely
set into countersink of eave gusset
plate assembly
109
8